Nickel-chromium (Ni-Cr) porcelain-fused-to-metal (PFM) crowns are widely used in prosthodontics due to their cost-effectiveness and favorable mechanical properties. As a classic metal-ceramic restoration, they consist of a nickel-chromium alloy substructure and a veneered porcelain layer that mimics natural tooth color.
The Ni-Cr alloy core provides excellent strength and rigidity, ensuring the restoration resists occlusal forces and avoids deformation, making it suitable for posterior teeth with heavy chewing loads. Compared with precious metal alloys like gold, Ni-Cr alloys are more economical, which is a key advantage for patients with budget constraints.
However, Ni-Cr PFM crowns have limitations. A small percentage of patients may experience allergic reactions to nickel ions released from the alloy, leading to gingival inflammation or discoloration. In addition, the metal substructure may cause a grayish gingival margin over time due to metal ion deposition, affecting aesthetic outcomes, especially for anterior teeth.
Clinically, Ni-Cr PFM crowns require precise fabrication: technicians must ensure uniform porcelain thickness and proper metal-ceramic bonding to prevent porcelain chipping. They remain a mainstream restoration option in dental clinics, balancing functionality, aesthetics and affordability for edentulous defect repair.